How fast should china paints be fired?

Overglazes can usually be fired and cooled rapidly. The exception is pieces with uneven thicknesses, such as a vase with thin walls and a thick base. In general, fire china paints 2 - 2 ½ hours.

Try adding a 20-minute “hold” or “soak” to the ... [More]

What causes purple spots in gold glaze?

Purple spots in gold can be caused by overfiring or by too heavy an application. However, this is very attractive when gold is crackled over a dark color of fired glaze.

... [More]

Showing FAQs 2of 2    


Paragon Kilns on FacebookParagon Kilns on Twitter Paragon Kilns on YouTube Paragon RSS Feed

Kilns Sold

Get The Adobe Reader

Home

  • Home
  • Privacy Statement
  • Legal Notice
  • Paragon's Green Statement
  • Where To Buy Kilns
  • Resellers
  • About Us
  • Contact Paragon
  • News & Events
  • Support

  • Kiln Technicians
  • Kiln Support
  • Products

  • Bead Kiln
  • Glass Blower's Crucible Furnace
  • Ceramic Kilns
  • China Painting Kilns
  • Enameling Kilns
  • Industrial Furnaces
  • Glass Kilns
  • Lamp Working Kilns
  • Pottery/Ceramic and Glass
  • Pottery Kilns
  • Silver Clay Kilns
  • Wax Burnout Furnaces
  • Heat Treating Ovens
  • Knife Making Ovens
  • Custom Furnaces
  • Discontinued Models
  • “Custom and standard Kilns and Industrial Furnaces for ceramics, pottery, heat treating, enameling,
    dentistry, laboratory, and glass fusing.
    Better Designed Kilns from Paragon Industries!"